Título : Avaliação da resistência de união entre uma cerâmica feldspática e três ligas metálicas alternativas
Autor(es): Vilela Neto, Evandro
Orientador: Reskalla, Helcio Nagib José Feres
Co-orientador: Leite, Fabíola Pessôa Pereira
Miembros Examinadores: Concílio, Laís Regiane da Silva
Resumo: Este estudo avaliou, in vitro, a resistência de união ao cisalhamento entre uma cerâmica feldspática (VITAVM®13) e três ligas metálicas a base de Ni-Cr (Wironia Light®), de Ni-Cr-Ti (Tilite®) e de Co-Cr (Wirobond 280®), visando identificar a liga que apresenta os maiores índices de resistência à fratura no sistema metalocerâmico em que foram constituídos três grupos (n = 10): G1 (controle) – Ni-Cr/cerâmica; G2 – Ni-Cr-Ti/cerâmica; G3 – Co-Cr/cerâmica. Os trinta corpos de prova confeccionados, a partir de padrões de cera cilíndricos com 15 x 6 mm que foram obtidos por meio de matriz metálica, em que cada liga foi fundida conforme orientações de cada fabricante, utilizando-se a técnica da cera perdida. O acabamento foi realizado e em seguida os espécimes foram jateados com Al2O3. A quantidade da cerâmica aplicada foi padronizada utilizando-se a porção superior móvel da matriz, em forma semicircular de 3 mm de altura, que apresenta um orifício de 8,4 mm de diâmetro proporcionando camadas de cerâmica com dimensões semelhantes em todos os corpos de prova. Na investigação, foi utilizado o teste de cisalhamento, e durante o ensaio foram obtidos valores de força máxima de tensão (MPa) e deformação específica (%). Os padrões de falhas ocorridas (adesiva, coesiva ou mista) foram observados em estereomicroscópio. Ao MEV foram observadas, de forma descritiva, as superfícies fraturadas no teste ao cisalhamento e, ao EDS, de forma quantitativa (%), os elementos químicos. Para estas análises foram selecionadas, de forma aleatória, três corpos de prova de cada grupo. Na análise estatística aplicou-se ANOVA, prova de Kolmogorov-Smirnov, prova de Levene, prova robusta de Brown-Forsythe, prova do Qui-Quadrado e teste de Post-Hoc de Fisher's Least Significant Difference, todos com nível de significância de 5%. Ao teste de cisalhamento obteve-se as seguintes médias de tensão (MPa): G1 = 31,22 ± 7,06; G2 = 21,13 ± 4,02, e; G3 = 23,02 ± 5,69. Já as médias de deformação (%) foram: G1 = 12,28 ± 2,95; G2 = 7,948 ± 3,05; G3 = 9,19 12,28 ± 5,90. Na comparação entre os grupos, no teste de cisalhamento, no que se refere à força de tensão, identificou-se que G1 (Ni-Cr) se diferenciou estatisticamente de G2 (p = 0,002) e de G3 (p = 0,013). Com relação aos elementos químicos encontrados nas superfícies dos espécimes analisados observou-se as seguintes diferenças estatisticamente significantes: no metal – G1 x G2 (Cr: p = 0,004); G1 x G3 (Co: p = 0,000; Ni: p = 0,041; W: p = 0,000); G2 x G3 (Co: p = 0,000; Cr: p = 0,0005; W: p = 0,000), e; na cerâmica – G1 x G2 (Al: p = 0,005; O: p = 0,010; Si: p = 0,005) e G2 x G3 (Al: p = 0,027; Si: p = 0,016). As ligas Ni-Cr e Co-Cr apresentaram 100% de falhas mistas. Já a liga Ni-Cr-Ti apresentou falhas mista (60%) e adesiva (40%). Portanto, conclui-se que todas as ligas estudadas estão indicadas para uso clínico; no entanto, a liga à base de Ni-Cr foi a que apresentou maior média de resistência de união, ao cisalhamento, com a cerâmica feldspática.
Resumen : This study in vitro evaluated the bond shear strength from a feldspathic ceramic (VITAVM®13) and three Ni-Cr alloys (Wironia Light®), Ni-Cr-Ti (Tilite®) and Co-Cr (Wirobond 280®), to identify the alloy has the highest fracture resistance levels in metal-ceramic system in which they were constituted three groups (n = 10): G1 (control) – Ni-Cr/ceramics; G2 – Ni-Cr-Ti/ceramics; G3 – Co-Cr/ceramic. The thirty specimens confectioned from cylindrical wax patterns with 15 x 6 mm that were obtained by means of metallic matrix, wherein each league was fused according to guidelines of each manufacturer, using the lost wax technique. The finish was conducted and then the specimens were sandblasted with Al2O3. The amount of the ceramic applied was standardized using the movable upper portion of the die in circulate-half shape 3 mm in height, having a hole of 8.4 mm diameter providing ceramic layers with similar dimensions in all specimens. In the investigation, the shear test was used, and during the test were obtained maximum voltage values of strength (MPa) and specific strain (%). The patterns of faults occurred (adhesive, cohesive or mixed) were observed in stereo. When SEM were observed in a descriptive way, the fractured surfaces in shear test and when EDX, quantitatively (%), the chemical elements. For these analyzes were selected, at random, three specimens of each group. ANOVA, Kolmogorov-Smirnov test, Levene proof, Brown-Forsythe robust proof, Chi-Square and Post-Hoc test Fisher's Least Significant Difference was applied in statistical analysis, all with significance level of 5%. In the shear test there was obtained the following stress average (MPa): G1 = 31.22 ± 7.06; G2 = 21.13 ± 4.02, and; G3 = 23.02 ± 5.69. Since the strain, average (%) were: G1 = 12.28 ± 2.95; G2 = 7.948 ± 3.05; G3 = 9.19 12.28 ± 5.90. In comparison between groups, in shear testing, with regard the tensile strength, it was identified that G1 (Ni-Cr) G2 differed statistically (p = 0.002) and G3 (p = 0.013). With respect to the chemical elements found on the surfaces of the specimens analyzed, we observed the following significant differences: the metal in metal – G1 x G2 (Cr: p = 0.004); G1 x G3 (Co: p = 0.000; Ni: p = 0.041; W: p = 0.000); G2 x G3 (Co: p = 0.000; Cr: p = 0.0005; W: p = 0.000), and; ceramics – G1 x G2 (Al: p = 0.005; O: p = 0.010; Si: p = 0.005) and G2 x G3 (Al: p = 0.027; Si: p = 0.016). Ni-Cr and Co-Cr alloys showed 100% of mixed failures. Since the Ni-Cr-Ti had mixed failure (60%) and adhesive (40%). Therefore, it is concluded that all the alloys studied are indicated for clinical use; however, to basis Ni-Cr showed the highest mean bond strength, shear, with feldspathic ceramic.
Palabras clave : Cerâmica.
Metais
Ligas metalocerâmicas
Resistência de materiais
Microscopia eletrônica de varredura
Ceramics
Metals
Metal-ceramic alloys
Material resistance
Scanning electron microscopy
CNPq: CNPQ::CIENCIAS DA SAUDE::ODONTOLOGIA::CLINICA ODONTOLOGICA
Idioma: por
País: Brasil
Editorial : Universidade Federal de Juiz de Fora (UFJF)
Sigla de la Instituición: UFJF
Departamento: Faculdade de Odontologia
Programa: Programa de Pós-graduação em Clínica Odontológica
Clase de Acesso: Acesso Aberto
URI : https://repositorio.ufjf.br/jspui/handle/ufjf/4543
Fecha de publicación : 2-jul-2015
Aparece en las colecciones: Mestrado em Odontologia (Dissertações)



Los ítems de DSpace están protegidos por licencias Creative Commons, con todos los derechos reservados, a menos que se indique lo contrario.