Avaliação da resistência da união de sistemas adesivos após a aplicação de agentes dessensibilizantes em dentina humana
Loading...
Date
Journal Title
Journal ISSN
Volume Title
Publisher
Universidade Federal de Juiz de Fora
DOI
Abstract
The aim of study was evaluate the microtensile bond strength of the total etch (Single
Bond II, SB) and self-etch adhesive systems (Clearfil SE Bond, SE) in human dentin
after desensitizer agents. Disks were obtained from human third molars, which had
their oclusal enamel removed to expose flat dentin surface. Six groups were formed
according to the materials used: G1 (control)- hybridization with SB, G2- oxalate
desensitizer (BisBlock, BB) and SB, G3- fluoride desensitizer (Aqua Prep F, AF) and
SB, G4 (control)- hybridization with SE, G5- BB and SE, G6- AF and SE. On these
surfaces were made blocks of composite Filtek Z350 of 5 mm to obtain “sticks”
10x1x1 mm. The specimens were stored in deionized water at 37°/ 24 h and
subjected to microtensile testing 1 mm/min until fracture. The images were observed
in MEV. The results were analyzed ANOVA two-way and Tukey test (p<0,05). The
mean values of the groups in MPa were: G2- 46.48(8.04), G3- 44.87(11.26), G5-
39.02 (13.45), G4-36.95(7.14), G1- 36.66(10.84) and G6- 32.71(13.83) which
showed no statistically significant difference between groups (p =0.012). It can be
concluded that the combined use the desensitizers and adhesive systems in human
dentin etched there is no influence on bond strength.
Description
Citation
Collections
Endorsement
Review
Supplemented By
Referenced By
Rights and licensing
Acesso Aberto