The aim of study was evaluate the microtensile bond strength of the total etch (Single Bond II, SB) and self-etch adhesive systems (Clearfil SE Bond, SE) in human dentin after desensitizer agents. Disks were obtained from human third molars, which had their oclusal enamel removed to expose flat dentin surface. Six groups were formed according to the materials used: G1 (control)- hybridization with SB, G2- oxalate desensitizer (BisBlock, BB) and SB, G3- fluoride desensitizer (Aqua Prep F, AF) and SB, G4 (control)- hybridization with SE, G5- BB and SE, G6- AF and SE. On these surfaces were made blocks of composite Filtek Z350 of 5 mm to obtain “sticks” 10x1x1 mm. The specimens were stored in deionized water at 37°/ 24 h and subjected to microtensile testing 1 mm/min until fracture. The images were observed in MEV. The results were analyzed ANOVA two-way and Tukey test (p<0,05). The mean values of the groups in MPa were: G2- 46.48(8.04), G3- 44.87(11.26), G5- 39.02 (13.45), G4-36.95(7.14), G1- 36.66(10.84) and G6- 32.71(13.83) which showed no statistically significant difference between groups (p =0.012). It can be concluded that the combined use the desensitizers and adhesive systems in human dentin etched there is no influence on bond strength.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By

Rights and licensing

Acesso Aberto