A utilização de um primer autocondicionante como alternativa ao ácido fluorídrico gera vantagens mecânicas e superficiais em cerâmicas vítreas?
Loading...
Date
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
Universidade Federal de Juiz de Fora (UFJF)
Abstract
Objective: This study evaluated the use of a self-etching primer as an alternative
to hydrofluoric acid, given the resistance to biaxial bending, roughness and
surface topography of lithium disilicate ceramics and those infiltrated by
polymers. Methodology: Fifty-four discs (:12mm; thickness: 1.2mm – ISO
6872) were made from two ceramics: IPS e.max CAD (LD – Ivoclar) and Enamic
(ceramic infiltrated by polymer – Vita). The samples were randomly distributed
into 3 groups, according to the “surface treatment” factor (n = 18 / with n=15, for
mechanical tests and n=3, for complementary tests): HF20 - 5% hydrofluoric acid
+ silane, applied for 20s; HF60 - 5% hydrofluoric acid + silane, applied for 60s;
and P - Self-etching ceramic primer. After surface treatment, the discs were
cemented in a dentin analogue (G10), which was prepared with a self-etching
universal adhesive and, after mechanical cycling (1.2x106 cycles, 50N, 3.8Hz)
and subjected to biaxial bending. (EMIC, DL, 1000-1mm/min, 1,000 Kgf).
Profilometry, SEM and EDS were also performed as complementary tests. The
biaxial flexural strength and roughness data were subjected to analysis of
variance (1-factor ANOVA) and the Tukey test (5%). Weibull analysis was
performed for biaxial flexural strength data. Results: According to ANOVA, it can
be observed that the surface treatment did not significantly influence the biaxial
flexural strength of both ceramics: LD (p=0.5552) and PIC (p=0.5205). Despite
the manufacturer's instructions regarding the use of HF20 for PIC ceramics, it
appears that there was no significant difference in biaxial resistance in the HF60
groups (1240 ± 161 A) compared to the HF20 (1246 ± 207.7 A) and the P (1306 ±
143.3 A). The same can be true for the LD group, where both groups predispose
without significant differences. Conclusion: surface treatment did not
significantly influence the biaxial flexural strength for the ceramics evaluated. A
similarity was observed in relation to biaxial flexural strength when etching with
5% hydrofluoric acid for 20, 60 seconds and self-etching primer, in relation to
lithium disilicate ceramics and polymer infiltrated ceramics.
Description
Keywords
Citation
Collections
Endorsement
Review
Supplemented By
Referenced By
Creative Commons license
Except where otherwise noted, this item's license is described as Acesso Aberto