A utilização de um primer autocondicionante como alternativa ao ácido fluorídrico gera vantagens mecânicas e superficiais em cerâmicas vítreas?

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

Universidade Federal de Juiz de Fora (UFJF)

Abstract

Objective: This study evaluated the use of a self-etching primer as an alternative to hydrofluoric acid, given the resistance to biaxial bending, roughness and surface topography of lithium disilicate ceramics and those infiltrated by polymers. Methodology: Fifty-four discs (:12mm; thickness: 1.2mm – ISO 6872) were made from two ceramics: IPS e.max CAD (LD – Ivoclar) and Enamic (ceramic infiltrated by polymer – Vita). The samples were randomly distributed into 3 groups, according to the “surface treatment” factor (n = 18 / with n=15, for mechanical tests and n=3, for complementary tests): HF20 - 5% hydrofluoric acid + silane, applied for 20s; HF60 - 5% hydrofluoric acid + silane, applied for 60s; and P - Self-etching ceramic primer. After surface treatment, the discs were cemented in a dentin analogue (G10), which was prepared with a self-etching universal adhesive and, after mechanical cycling (1.2x106 cycles, 50N, 3.8Hz) and subjected to biaxial bending. (EMIC, DL, 1000-1mm/min, 1,000 Kgf). Profilometry, SEM and EDS were also performed as complementary tests. The biaxial flexural strength and roughness data were subjected to analysis of variance (1-factor ANOVA) and the Tukey test (5%). Weibull analysis was performed for biaxial flexural strength data. Results: According to ANOVA, it can be observed that the surface treatment did not significantly influence the biaxial flexural strength of both ceramics: LD (p=0.5552) and PIC (p=0.5205). Despite the manufacturer's instructions regarding the use of HF20 for PIC ceramics, it appears that there was no significant difference in biaxial resistance in the HF60 groups (1240 ± 161 A) compared to the HF20 (1246 ± 207.7 A) and the P (1306 ± 143.3 A). The same can be true for the LD group, where both groups predispose without significant differences. Conclusion: surface treatment did not significantly influence the biaxial flexural strength for the ceramics evaluated. A similarity was observed in relation to biaxial flexural strength when etching with 5% hydrofluoric acid for 20, 60 seconds and self-etching primer, in relation to lithium disilicate ceramics and polymer infiltrated ceramics.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By

Creative Commons license

Except where otherwise noted, this item's license is described as Acesso Aberto