Efeito de diferentes soluções na limpeza sônica dos precipitados do ácido fluorídrico sobre a resistência de união entre uma cerâmica feldspática e um cimento resinoso

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

Universidade Federal de Juiz de Fora (UFJF)

DOI

Abstract

The objective of this study was to evaluate the hypotheses: different ultrasonic cleaning media of the hydrofluoric acid precipitates influence the values of union resistance between ceramic feldspatic and resinous cement. Twenty blocks of Vita VM7 ceramic (VITA ® ) were obtained. The cementation surface of each block was duplicated in resin composite (W3D ® ). Ceramic blocks were randomly assigned in to 4 groups (n = 5/per group): G1 – etching with 9,6% AFL (Dentsply ® ) for 20s + rinsing with water spray for 60s + drying (Control); G2 – 9,6% AFL for 20s + rinsing with water spray for 60s + ultrasonic cleaning (Vitasonic ® ) in distilled water for 4 min + drying; G3 – 9,6% HF for 20s + rising with water spray for 60s + ultrasonic cleaning in acetone 99,5% 4 min + drying; G4 – 9,6% AFL for 20s + rinsing with water spray for 60s + ultrasonic cleaning in alcohol 70% for 4 min + drying . The ceramic blocks were silanized Porcelain Primer (Dentsply ® ) and cemented to the composite blocks using the resin cement RelyXTM ARC. The cemented blocks were sectioned in to axes (X and Y) with a diamond disk under coolant irrigation in order to obtain microbars with 1,0 mm² of bonding area. Each bar was attached to an adapted device and the microtensile test was performed using a universal testing machine (crosshead speed: 1 mm/min. The bond strengths and SD in Mpa were as follows: G1) 16,60 ± 0,52a; G2) 18,75 ± 0,37b; G3) 16,09 ± 0,92a e; G4)15,75 ± 1,38a. Utrasonic cleaning media after etching resulted in signifant difference among the groups (p < 0,05) (One-way ANOVA and Tuckey test). Only ultrasonic cleaning in distilled water demonstrated the highest bon strength with the tested resin-cement to feldspatic ceramic. Ultrasonic cleaning in acetone 99,5% and alcohol 70% did not affect the bond results.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By

Rights and licensing

Acesso Aberto