Abstract
The preheating of composite resins is widely employed to improve their physical and
chemical properties, such as reducing viscosity and increasing the degree of
monomer-to-polymer conversion. However, repeated application of preheating cycles
may lead to thermal degradation of the resin components, especially in bulk-fill
materials. This study evaluated the effect of 10 preheating cycles at 68°C on the
degree of conversion and surface microhardness of bulk-fill resins (regular and
flowable). The degree of conversion (%) was analyzed by Fourier Transform Infrared
Spectroscopy (FTIR), using a PerkinElmer Spectrum Two™ spectrometer with an ATR
device and a ZnSe crystal. Samples were photoactivated for 20 seconds using an LED
light source (1,100 mW/cm²) and analyzed in the range of 1750–1550 cm⁻¹.
Calculations were based on the intensity of the C=C double bond (1636 cm⁻¹) and the
aromatic ring stretch (1600 cm⁻¹ for the regular resin and 1608 cm⁻¹ for the flowable
resin) as the internal standard. Vickers microhardness (HV) was evaluated using
cylindrical specimens (5 mm in diameter and 2 mm in thickness), which were
photoactivated and polished. Three indentations per sample were performed (50 g for
45 seconds), and values were calculated using the equation VH = P/2d². The results
showed no significant differences in the degree of conversion (%) or microhardness
(HV) after the preheating cycles, indicating that the tested resins have stable
formulations and are resistant to multiple thermal exposures. The preheating technique
appears to pose no apparent risk of degradation for the evaluated resins. However,
thermal stability may vary among different formulations, highlighting the need for
further studies evaluating the impact of preheating cycles on a broader range of
materials and under long-term clinical conditions.
Description
Keywords
Resinas Compostas , Polimerização , Dureza , Espectroscopia de Infravermelho com Transformada de Fourier , Testes Mecânicos , Pré-aquecimento de resinas compostas , Composite Resins , Polymerization , Hardness , Fourier-Transform Infrared Spectroscopy , Mechanical Testing , Preheating of composite resins
Citation
Collections
Endorsement
Review
Supplemented By
Referenced By
Creative Commons license
Except where otherwise noted, this item's license is described as Acesso Aberto