Estudo do potencial de aplicação de resíduo de concreto em substituição ao agregado graúdo para concretos permeáveis
Loading...
Date
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
Universidade Federal de Juiz de Fora (UFJF)
DOI
Abstract
The search for environmental preservation and conservation of natural resources, motivated by
the activities harmful to the environment associated with the construction industry, makes new
concepts and technical solutions viable for sustainable development. The genesis of the present
work derives precisely from the lack of financial resources that characterize the current
economic situation of brazilian universities, together with the growing demand for repairs in
the Federal University of Juiz de Fora buildings: to use the large amount of concrete waste
generated and deposited in areas of the Campus replacing natural aggregates in the production
of pervious concrete, which, in turn, represents an excellent artifice in the fight against the
phenomenon of urban surface waterproofing. There are numerous benefits of using permeable
coatings in paving: reduce runoff; temporarily storing the surplus water, relieving the drainage
system; to feed the underground aquifer and recover the soil filtration capacity; in addition to
presenting lower life cycle cost in detriment to other conventional materials. This research
involves the pioneering assessment about the influence of the use of these recycled waste in
replacement to 100% of the conventional aggregate of stone origin in the mechanical and
hydraulic behavior of the pervious concrete by means of tests recommended by ABNT NBR
16416: 2015, without the use of additives. For that, a dosage study was carried out to determine
the most suitable trait for the preparation of the drainage composite as a floor, and it was hoped
to obtain a material in accordance with the normative requirements of resistance and
permeability, from technically feasible procedures. All the permeability coefficients obtained
in the laboratory exceeded the normative limit of 0.1 cm/s, reaching values of up to 2.36 cm/s.
Likewise, average compressive strength values of the test pieces close to the limit of 20 MPa
stipulated by the standard (23.98 MPa and 19.57 MPa for 60 mm and 80 mm pieces
respectively) were obtained and the flexural tensile strength was also observed: mean of 2.08
MPa, higher than the recommended minimum (2 MPa). In view of the favorable outlook, the
final products can be manufactured in series by the institution and used in the maintenance of
the Campus areas, directly and indirectly reducing the expenses associated with the construction
waste and the waterproofing of the urban pavements.