Resistência da união ao teste de push-out de cimentos resinosos auto-adesivos em dentina radicular

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

Universidade Federal de Juiz de Fora

DOI

Abstract

This study evaluated the push-out bond strength of two self-adhesive resin cements and a conventional etch-and-rinse resin cement on root dentin. Sixty human third molars were endodontically treated and a glass fiber post was cemented with one of three resin cements. Each root was cut transversely to obtain three slices (dentin-post) of 1 mm thick. The slices of the cervical, middle and apical root canal were stored in deionized water at 37 °C for 24 hours or 30 days. After storage, the push-out test was performed. The values of bond strength were evaluated by ANOVA three way and Tuckey’ test (p = 0,05) and the types of fracture were evaluated by scanning electron microscopy. The bond strength of the self-adhesive resin cement RelyX U100 was superior to the RelyX ARC etch-and-rinse cement, after the two storage periods (p > 0.05). The analysis of 24 hours showed that at the cervical third, the values of bond strength of RelyX ARC were higher than that of the middle and apical thirds (p < 0.05). After 30 days of storage, the values at the three root thirds did not differ. The values of RelyX U100, on the three regions of the root canal did not differ, in both evaluations (p > 0.05). After 24 hours, BisCem showed higher bond strength at the apical third, followed by cervical. After 30 days, the values of bond strength at the three root thirds did not differ (p > 0.05). RelyX U100 did not exhibit changes in bond strength values after 30 days of storage (p > 0.05). BisCem showed no differences in the values obtained after 24 hours and 30 days of aging at the cervical and middle thirds (p > 0.05). The storage time of 30 days reduced the values of bond strength at the three root thirds of RelyX ARC. RelyX U100 e BisCem had the highest number of cohesive failures of the zone of interaction. RelyX ARC presented a higher number of cohesive failures of the hybrid layer were observed. It was concluded that the RelyX U100 self-adhesive resin cement showed higher bond strength than the conventional resin cement RelyX ARC, on the three root thirds, in both periods. BisCem showed bond strength comparable to RelyX U100. The storage time for 30 days caused changes on the bond strength of the RelyX ARC and BisCem resin cements.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By

Rights and licensing

Acesso Aberto