Abstract
The increasing incorporation of additive manufacturing into Dentistry has expanded the use of
three-dimensional (3D)-printed resin composites for the fabrication of permanent indirect
restorations. The aim of this study was to evaluate the microshear bond strength (µSBS) of a
universal dual-cure resin cement to the surface of a 3D-printed resin composite subjected to
different surface treatment protocols. Twenty-four discs of a 3D-printed resin composite
(Prizma 3D Bio Crown) (n=24) were fabricated and allocated into four experimental groups (n
= 6): OAL (50-µm aluminum oxide air abrasion); OBU (air abrasion + universal adhesive); SIL
(air abrasion + Monobond Etch & Prime); and SILOBU (air abrasion + Monobond Etch &
Prime + universal adhesive). Four cylinders of Maxcem Elite Universal resin cement were built
on each disc and submitted to a microshear bond strength test using a universal testing machine.
Failure modes were analyzed under a stereomicroscope and classified as adhesive, cohesive, or
mixed. Data were analyzed using one-way analysis of variance (ANOVA), followed by the
Games-Howell post hoc test (α = 5%). The SILOBU group exhibited the highest bond strength
values (23.6 ± 7.35 MPa), showing statistically significant differences compared with the OAL
(14.8 ± 3.38 MPa), OBU (15.4 ± 2.55 MPa), and SIL (12.6 ± 4.65 MPa) groups (p < 0.001),
whereas no significant differences were observed among the latter groups. Regarding the failure
pattern, mixed failures predominated (67.71%), followed by adhesive (18.75%) and cohesive
failures (13.54%). It was concluded that the combination of aluminum oxide air abrasion,
Monobond Etch & Prime, and universal adhesive significantly increased the bond strength
between the 3D-printed resin composite and the resin cement, demonstrating superior
performance compared with protocols based solely on mechanical or chemical surface
treatments.
Description
Citation
Collections
Endorsement
Review
Supplemented By
Referenced By
Creative Commons license
Except where otherwise noted, this item's license is described as Acesso Embargado