Verificação da existência de porosidade interna em duas resinas acrílicas termopolimerizáveis com diferentes volumes e métodos de processamento
Loading...
Date
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
Universidade Federal de Juiz de Fora (UFJF)
DOI
Abstract
This study used specimens with different volumes polymerized in heated
water with microwave energy and thermopneumohydraulic curing, in order to visually
verify the existence of internal porosity in the thermally activated acrylic resins Clássico® and Onda Cryl®. To make the 60 specimens, which were divided randomly
into three groups with different volumes (n = 5), measuring respectively, 4 X 3cm, 3 X
2cm, 1 X 2cm and 3 X 10 X 0.3cm, acrylic resins were handled following the
manufacturer's recommendations and positioned manually in flasks in its plastic
phase. Then the flasks were brought to hydraulic press for a period of 08 hours and
placed in a humidor at 37ºC. For processing by microwave energy, was used cycle
40% power for 03 minutes, 0% power for 04 minutes and 90% power for 03 minutes.
In the conventional, the specimens were polymerized in heated water bath for 09
hours at a temperature of 74ºC and thermopneumohydraulic, flasks were placed in a
thermal curing in pressure of 20 pounds to the temperature of 120ºC, followed by
cooling to 90ºC, and again increased to 120ºC for 40 minutes. All flasks processed at
the three methods were kept in room temperature until the complete cooling. After
polymerization and unflanking, the specimens were finished and polished. To check
the porosity, three observers used predetermined scores: "0" – no pore, "1" – pores
in minimal amount, "2" – pores in greater quantity, "3" – pores occupying a large part
of total and "4" – pores in the total volume. The data were subjected to Kruskal-Wallis
and Mann-Whitney tests with a significance level of 5% (p
≤ 5). The score "0" was
more frequent with 37.8% followed by the score "1" with 31.1%.
A statistically
significant difference between the scores and the sizes of the specimens (p = 0.023)
was observed. The average percentage of the scores assigned to the specimens
according to the method of polymerization reached 37.8%. There were no statistically
significant differences between processing methods, however the “p” hit 0.593. It can
be concluded that the specimens showed great score "1" and the average score "3",
the samples were small and laminar score "1" and "0" respectively. The three
polymerization methods used were similar, with no statistically significant difference
between them in two acrylic resins tested. Regardless of the method of processing,
the internal porosity was directly proportional to the volume of specimens.
Description
Keywords
Resinas acrílicas , Porosidade , Micro-ondas , Pressão , Acrylic resins , Porosity , Microwave , Pressure