This work has as objective a ceramic crucible confection with complete functionality
for use in Industrial Processes Laboratory at UFJF and also for a confection method study
in order to provide future copies if necessary. The adopted confection method is Slip
Casting method, which uses a porous cast and a slip. The porous cast is obtained through
a mixture containing plaster and water, while the slip is obtained through a mixture of
water, kaolin and a deflocculant agent. The porous cast was obtained through a mixture of
approximately 40% water and 60% plaster (in weight), while the suspension was obtained
through a mixture of 400ml water, 100ml kaolin and 4 drops of deflocculant agent. The
Slip Casting method consists of filling a porous cast with a slip mixture, in which the liquid
part from the slip is absorbed by the casts’ pores, forming a clay layer near the cast’s walls
with varying thickness according to the casting’ duration. After the clay wall is formed,
the slip’s excess must be removed. The absorbing time was 1min for the smaller casts and
2min for the bigger casts. The cast and clay coating must go through a drying period
until the clay coating can be properly taken off. After dried the clay coating has the final
product’s dimensions. After the casting process the product must go through sintering in
a furnace at approximately 1300 C, but the rapid temperature increase during sintering
could lead to structural defects causing deformations and possible cracks. In order to
avoid said problems, a programmable temperature ramp furnace was used, initially heating
until 400 C at a 5 C/min rate and remaining at the final temperature for 30min, then
heating at a 12 C/min rate until 1000 C, remaining there for 2h. Even without cautious
air removal from the slip, the casting slip process was efficient for small sized crucibles.
However, for bigger crucible dimensions the structural failures caused by air bubbles made
the sintering process impossible.
Description
Keywords
Citation
Collections
Endorsement
Review
Supplemented By
Referenced By
Creative Commons license
Except where otherwise noted, this item's license is described as Acesso Aberto