Avaliação da influência do tratamento térmico do silano sobre a resistência de união entre cimentos resinosos e uma cerâmica feldspática

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

Universidade Federal de Juiz de Fora

DOI

Abstract

The aim of this study was to evaluate three hypotheses: H0- Heat treatment of silane and resin cement type does not influence the bond strength of resin cements and a feldspathic ceramic;H1- Heat treatment of silane influences the bond strength between cements resin and a feldspathic ceramic; H2- The resin cement influences the bond strength of a feldspathic ceramic. Thirty blocks were fabricated using a ceramic (VITA Mark II, Zahnfabrik), which were duplicated in composite resin (W3D Master, Wilcos). The blocks were divided into 6 groups (n = 5) in accordance with the following surface treatments: ASCp- Hydrofluoric acid 10% + silane + Panavia F; ASTCp- Hydrofluoric acid 10% + silane + heat treatment (furnace) + Panavia F; STCp- Silane + heat treatment (furnace) + Panavia F; ASCr- Hydrofluoric acid 10% + silane + RelyX ARC; ASTCr- Hydrofluoric acid 10% + silane + heat treatment (furnace) + RelyX ARC; STCr- Silane + heat treatment (furnace) + RelyX ARC. To perform the heat treatment silane was used furnace under temperature of 100 ° C for 2 minutes. Then each ceramic block conditioning was already attached to its corresponding composite resin, using a resin cement to its respective group, under the constant load of 750g. Each set ceramic / cement / composite resin was sectioned and the specimens were analyzed by microtensile mechanical test. The bond strength values and standard deviations (MPa) for the groups were: ASCp (25.47 ± 9.34a); ASTCp (33.04 ± 10.65b); STCp (13.76 ± 8.82c); ASCr (24.80 ± 7.99a); ASTCr (23.84 ± 7.16a); STCr (11.41 ± 11.71c). ANOVA and Post Hoc were applied. With the results of this study, we can conclude: The hypothesis H0 was rejected; H1 hypothesis was partially accepted because the heat treatment of the silane led to the highest average bond strength provided it is conducted in association with the hydrofluoric acid etching 10%, independent of the resin cement tested; H2 hypothesis was partially accepted because the cement with MDP averaged bond strength statistically superior to conventional cement when the conditioning was conducted with 10% hydrofluoric acid prior to the heat treatment of silane.

Description

Citation

Endorsement

Review

Supplemented By

Referenced By

Rights and licensing

Acesso Aberto