Abstract
In this work, Ag nanoparticles and bimetallic nanoparticles of Ag-Au and Au-Ag on
polyaniline (PANI) nanofibre films were prepared. Each stage of the work was
characterized using UV-VIS-NIR absorption and Raman spectroscopies, and scanning
and transmission electron microscopies. The analysis of the composition of the bimetallic
nanoparticles was performed by energy dispersion using the X-ray spectroscopy.
PANI nanofibers doped with HCl were synthesised via a fast mixture of ammonium
persulfate and aniline precursors. These nanofibers of esmeraldine salt (ES), which have
an average thickness of 27 nm, were immersed in a basic solution for the deprotonation
and formation of the base of esmeraldine base (EB). Bare glass substrates and modified
glass substrates prepared by immersion in H2SO4/H2O2 and H2O/H2O2/NH4OH solutions,
were used for the deposition of nanofibers, through immersion in the suspension of the
ES, forming thin films of PANI. Thick films were also prepared by dripping the
suspension of the PANI on the glass slide. In addition to the film doped with HCl, films
doped with citric acid, phosphoric acid, mandelic acid, and toluene sulfonic acid were
also prepared.
The films of ES doped with the different acids and the EB film were immersed in AgNO3
solution for the reduction of Ag+ ions and formation of silver nanoparticles. It was noticed
that the size and shape of the silver nanoparticles strong depend on the dopant and the
thickness of the ES film. It was observed the formation of nano and microstructures in
the range of 2 to 370 nm with shapes of needles, spheres, plates, and wires.
The thin and thick films doped with HCl containing silver nanoparticles were
subsequently immersed in HAuCl4 solution for the formation of bimetallic nanoparticles
Ag-Au. It was also prepared bimetallic nanoparticles Au-Ag onto the films doped with
HCl (thin and thick films) first by immersion in a gold salt solution and then immersion
in a silver salt solution. The structures formed presented cubical, spherical, medium-sized
wires in the range of 5 to 700 nm influenced by film thickness and synthesis mechanism.
In addition, modifications in the polymeric structure were observed indicating the
presence of phenazine, phenoxazine and safranin groups.