Abstract
Light-cured composite resins are essential materials in restorative dentistry, standing out
for their clinical versatility, adequate mechanical strength, good handling properties, and
satisfactory esthetics, which are provided by the wide range of available shades and
opacities. The effectiveness of these materials depends significantly on proper
polymerization. The degree of conversion and microhardness are critical mechanical
properties that determine the clinical performance of restorations. This study investigated
whether there is a statistically significant difference in the degree of polymerization
conversion and microhardness of composite resins with different shades (B1 and A3.5),
light-cured using the same photoinitiator under identical conditions of power, light
intensity, and activation time. This experimental comparative study included five
specimens for each composite resin shade. The specimens were standardized with
dimensions of 5 mm in diameter and 2 mm in thickness, molded using a silicone matrix
to form uniform cylindrical samples. Light curing was performed using a Bluephase G4
LED curing unit (Ivoclar Vivadent) for 20 seconds, applying a light intensity of 1200
mW/cm2. After polymerization, the specimens were sequentially polished using abrasive
papers of different grit sizes and analyzed by Fourier-transform infrared spectroscopy
(FTIR) to determine the degree of conversion, as well as by the Knoop microhardness
test. The data were statistically analyzed using the independent Student’s t test, with the
level of significance set at P < 0.05. The results showed that both groups exhibited high
degrees of conversion (B1: 80.90% ± 7.32% and A3.5: 82.46% ± 10.24%), with no
statistically significant difference between them (p = 0.789). Similarly, microhardness
values (B1: 119.3 ± 5.35 HK and A3.5: 112.2 ± 15.55 HK) did not differ significantly
between the groups (p = 0.365). These findings indicate that the shade of the composite
resin, within the evaluated tonalities, does not significantly influence either the degree of
conversion or microhardness when subjected to the same light-curing conditions.
Therefore, the mechanical performance of composite resins with different shades does
not present clinically relevant variations, allowing clinicians to prioritize esthetic criteria
when selecting the shade without compromising the mechanical properties of the
restoration.
Description
Keywords