Influência da barreira de proteção na capacidade de fotopolimerização de resinas bulk fill
Loading...
Date
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
Universidade Federal de Juiz de Fora (UFJF)
DOI
Abstract
The objective of this laboratory research was to evaluate whether the protection
barrier applied at the tip of the curing light interferes with the polymerization of
bulk fill resins. Four bulk fill resins (2 of regular consistency and 2 of fluid
consistency) were evaluated, in addition to a conventional resin (control group).
The samples were prepared in prefabricated matrices, with a resin insertion hole
measuring 6 mm in diameter x 2 mm in depth for the control group and 6 mm in
diameter x 4 mm in depth for the bulk fill resins, following the
photopolymerization indicated by the manufacturers. 300 specimens were
made, divided into 5 groups (60 specimens for each resin) polymerized by 3
photopolymerization devices of different commercial brands. Within each group,
20 specimens were polymerized by each curing light (10 specimens using the
protective barrier and 10 without its use). The specimens were submitted to the
top and bottom Knoop microhardness test and the results were statistically
analyzed by analysis of variance (ANOVA) with a significance level of 5%,
verifying that in the 5 groups the base/top ratio was significantly lower when the
protection barrier was used on the light-emitting tip of the curing light. Thus it is
concluded that the higher base/top ratio is directly linked to the better
performance of the curing light, indicating that in this study the disposable
protective barrier negatively influenced the light curing of bulk fill resins.
Description
Keywords
Citation
Collections
Endorsement
Review
Supplemented By